Nickel-based single crystal superalloys have been widely used in modern aircraft, which is related to its high temperature mechanical strength and creep properties. And the initial cubic γ′ precipitates start to coarsen directionally during high temperature creep, which results in the degradation of the mechanical properties, especially the creep properties. Therefore, it is essential to figure out the mechanism of directional coarsening during the period of high temperature creep. In this article, a broad review of rafting mechanism of nickel-based single crystal superalloys is provided. The major work of this critical review is to introduce several experiments and numerical simulations which are used to analyze the evolution of rafting. For three different numerical simulations, their performance, advantage and disadvantage are discussed in detail. Through methods above, the effect on creep properties is summarized.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.