The present research work describes a facile and industrial-friendly procedure for producing high quality CuO nano-powder from a PLS of a low-grade chalcopyrite-ore bioleaching. The PLS containing lower than about 1gCu/L (obtained from the ore bioleaching) was used as the feed for the procedure in which firstly the iron and other impurities was removed from the PLS, and next the pure copper–ammonia complex was selectively formed from the PLS. Then, the complex was transformed to the precursor (Copper Hydroxide Sulfate Hydrate (Cu2.5(OH)3(SO4)·(H2O)2)) at the room temperature. Finally, the precursor was dried at 60°C overnight to obtain pure CuO nano-powder (average crystalline size of about 19nm). The results were confirmed by the characterization analyses: XRD, SEM/EDS, elemental mapping, TEM, FTIR, chemical analyses, and XRF.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.