Abstract
In order to utilize blast furnace slag resource at low cost, pollution-free, refinement and high value-added, a novel technical route was proposed to collaboratively produce zeolite and hydrotalcite-like compound. In this study, the changing property of slag in the treatment process was investigated and the thermodynamic and kinetic analyses of the leaching reaction were conducted to prove its feasibility. The silica gel and residue liquid were separated effectively from the slag. Then, 13X zeolite and hydrotalcite-like compound were successfully synthesized from water quenching blast furnace slag using hydrochloric acid treatment followed by hydrothermal method and co-precipitation method. The successful formation of 13X zeolite and hydrotalcite-like compound were obtained effectively with good surface morphology and crystal structure. Mass balance of the blast furnace slag utilization process was established. Meanwhile, these two samples exhibited good behavior of CO2 adsorption capacity and enjoyed a promising market prospect. The maximum adsorption capacities of 13X zeolite and hydrotalcite-like compound were 116.48 mg g−1 at 313 K and 149.63 mg g−1 at 873 K, respectively. Finally, the preliminary economic evaluation of the integrated system was conducted, and the economic benefit of 1 kg slag was about 1.281 $.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.