Abstract

Sm 3+ doped LaBMoO 6 phosphors were prepared by using the solid-state reaction method. The microstructure, morphology, chemical element composition, absorption, luminescent performance, decay life and thermal stability of Sm 3+ doped LaBMoO 6 samples were studied. Sm 3+ doped LaBMoO 6 phosphors mainly emit orange light at 596 nm with a decay lifetime of milliseconds under the excitation of 405 nm. The chromaticity coordinates of Sm 3+ doped LaBMoO 6 samples are located in the orange region, which also have great thermal stability. The Sm 3+ doped LaBMoO 6 phosphors can be used as orange-emitting materials in W-LED devices.