This paper studies a novel method for the preparation of mesophase pitches suitable as carbon fibre precursors. A series of thermally treated petroleum pitches with mesophase contents ranging from 10.8 to 52.2 vol.% was obtained from pitch A-240. Separation of the phases was initially attempted by hot filtration, a suitable method for separating the phases in thermally treated coal-tar pitches. Although filtration failed for the petroleum samples, the behaviour observed led to the development of a new separation method that consists in the sedimentation of the mesophase. This method, after optimisation, yielded pitches with mesophase contents up to 97 vol.%, which were easily spun into carbon fibres of reasonable mechanical properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.