In this study, a novel method was used to synthesize ß-TCP/HAP biphasic ceramic scaffold from natural cancellous bone. Bovine bone was calcined to remove the organic content. The remaining material was then soaked in P 2O 5 solution for different periods. P ions were doped into cancellous bone and reacted with hydroxyapatite (HAP) to produce ß-tricalcium phosphate (ß-TCP) at room temperature without any subsequent high-temperature heat treatment. By increasing the soaking time, the crystalline phase composition of the calcined bone gradually changed from HAP into a HAP/ß-TCP biphasic structure with different HAP/TCP ratios. The crystallite size of HAP and ß-TCP was smaller than 100 nm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.