Abstract

Solid-state composite polymer electrolyte PEO18LiTFSI-xDMSO (CPEx) are prepared by the casting process. An optimized freestanding electrolyte CPEx system yields a lithium ionic conductivity of 2.8×10-4 Scm-1 at 60 oC with x =1.32. The interfacial resistances of Li/CPEx and Li/CPEx/H-LAGP are examined. The interfacial resistance between CPE0 and lithium metal is reduced sharply by the addition of DMSO for CPE1.32 at 60 oC after storage about 35 days. The aqueous lithium air battery consists of Li/CPE1.32/H-LAGP electrode as a lithium protected electrode is successfully operated with LiCl saturated LiOH aqueous solution as electrolyte and Pt black as reference electrode at current density of 0.2 mAcm-1 at 60 oC.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.