Abstract Nano-sized WC was successfully synthesized on high surface area carbon by a novel carbothermal method wherein carbonization of mixture of hydroxypropyl cellulose (HPC) and K2WO4 at 800 °C resulted in the simultaneous formation of carbon and WC nano-particles. Different with the common carbothermal method, porous carbon was obtained by pyrolysis of hydroxypropyl cellulose and the reducing gas of H2 was not necessary.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.