The present study reports a new and original technique for obtaining nickel catalysts characterized by small metal crystallites. The catalysts were prepared on γ-Al2O3. The total surface of the carrier was 37.5 m2/g. The preservation of the appropriate procedure and conditions of preparation allow a large expansion of active nickel surface (mean crystallite size 2.0–3.0 nm) in spite of the quite hard conditions of reduction (773 K and 3 h).