Abstract

The deposition of Pd black on the surface of a Pd sheet electrode was carried out chemically using active hydrogen passing through the electrode, and the Pd black deposits were found to grow up three-dimensionally. The hydrogenation rate of 4-methylstyrene increased over 40 times by using the palladinized Pd sheet electrode. The increase in catalytic activity is thought to be due to the increase in reaction zone and appearance of new active sites.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.