Abstract

Zinc electroplating from non-cyanide alkaline solution is carried out in the presence of condensation product formed between DL-alanine (DLA) and glutaraldehyde. The bath constituents and bath variables are optimized through standard Hull cell experiments. The current efficiency and the throwing power are measured. High shift of potential towards more cathodic direction was observed in presence of addition agents. Corrosion resistance test reveals good protection of base metal by zinc coating obtained from the developed electrolyte. SEM photomicrographs show fine-grained deposit in the presence of condensation product. IR spectrum of the scraped deposit shows the inclusion of the condensation product in the deposit during plating. The consumption of brightener in the lab-scale is 6 mLL-1 for 1000 amp-hour.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call