In order to improve the oxidation behavior of carbon/carbon silicide carbide composites prepared by liquid silicon infiltration of carbon/carbon porous preforms, a multilayer coating of dense SiC alternated with porous Si–Mo was prepared by chemical vapor deposition combined with slurry painting. Oxidation test showed that weight loss of the coated sample was only 0.25% after 150 h oxidation in air at 1673 K. And the coated sample gained weight in the course of 46 cycles of thermal shock test between 1673 K and 373 K. The coating remained intact during the two kinds of tests and no obvious failure was found. The excellent oxidation protective ability and thermal shock resistance of the SiC/Si–Mo coating can be attributed to the alternated structure.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.