In order to characterise filiform corrosion on a commercial AA2024-T351 aluminium alloy, a detailed microscopical study using SEM and EDS was performed. One set of AA2024-T351 aluminium alloy samples was alkaline-cleaned and deoxidised and chromate conversion coated. Another set was alkaline-cleaned only. Both samples were similarly spray coated with a 42 μm clear polyurethane topcoat. Filaments were subjected to a range of specimen preparation techniques. Sections and top views examined by SEM revealed varying degrees of attack ranging from generalised etching without local attack to severe local attack in the form of pitting, resulting in grain etchout, grain boundary attack and subsurface etchout. EDS revealed the presence of chloride deep into the pits and the subsurface etchout.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.