Poly(l-lactic acid-b-ethylene oxide-b-l-lactic acid) (PLLA-b-PEO-b-PLLA) triblock copolymers were synthesized by a ring-opening polymerization. PLLA and PEO sequentially crystallized by slowly cooling (â2 °C/min) from the melt. In the resultant spherulitic morphology, the retardation of polarized light was additive, and the sign of the spherulite (negative) was preserved when the PEO crystallized within the framework established by the PLLA crystals. Homopolymer blends of PLLA and PEO having the same composition as the block copolymer showed similar optical behavior. However, the change in the optical retardation upon crystallization of the PEO was much greater for the triblock copolymer than for the blend. Upon heating, the small-angle X-ray scattering from both the triblock copolymer and homopolymer mixture showed a stepwise increase in the long period at âŒ60 °C, i.e., when the PEO crystals melted. For comparable volume fractions (ÏPLLA = 0.57), the increase in long period was greater for the triblock c...
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.