Abstract

A layer of silver was deposited on the surface of PA6 fiber fabric by electroless plating method to prepare silver/PA6 conductive fabric. The surface morphology and structure of the coating were analyzed by SEM and EDS. Electroless plating process conditions: 11 g/L silver nitrate, ammonia and sodium hydroxide appropriate preparation into 1.1% silver ammonia solution. Ingredients of reducing agent: glucose 10 g/L, tartaric acid 2 g/L, ethanol 100 ml/L, pH 11-13 was adjusted by adding 10 g/L sodium hydroxide solution, temperature 20-30 °C, reaction time 3min.The resistance of the preparation of silver/PA6 fabric is less than 1 Ω/cm, elemental silver content is 100%, the conductivity is excellent, and the electromagnetic radiation resistance is excellent.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.