ABSTRACTAn aluminium-containing medium manganese steel has been designed to undergo intercritical annealing followed by quenching in water and subsequent partitioning. Water quenching, replacing the quenching temperature (QT) between 150 and 300°C in conventional quenching and partitioning steels, is therefore adopted in QP alloys, in order to guarantee the precise QT in practice. The low intercritical annealing temperature of 750°C refines both ferrite and prior austenite grains into submicron size. The large fraction of ultra-fine ferrite, as well as the transformation-induced plasticity effect of retained austenite, improves the overall ductility of this water-quenched and partitioned steel. The alloy has achieved excellent mechanical properties of 1130 MPa ultimate tensile strength combined with 19.2% total elongation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.