Abstract

A bulk nanocrystalline Al–5 at.% Fe alloy was synthesized by mechanical alloying and spark plasma sintering. The alloy exhibited a very high compressive yield strength of 1 GPa with a plastic strain of 0.3. The alloy consists of coarse α-Al grains that form from powder boundaries and nanocrystalline regions composed of α-Al and Al6Fe phases. The combination of the coarse and nanoscale grains are considered to be the reason for the large plastic strain in such a high-strength material.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.