In this paper, a hardening model is developed for the cross-sectional nanoindentation of ion-irradiated materials. The model is based on the derivation of an average defect density within the formed plasticity affected region, which depends on the distribution of defect density in the irradiated region, indentation depth and distance from the irradiated sample surface. A succinct parameter calibration process is proposed by comparing the theoretical results with experimental data at a given indentation depth. A good agreement with experimental data can be achieved for both the fitted relationship between irradiation hardening and indentation distance from the irradiated sample surface under cross-sectional nanoindentation, and predicted hardness as a function of indentation depth under surface nanoindentation. Therefore, the rationality and accuracy of the proposed model are effectively verified. Based on the analysis of this proposed model, it is available to characterize the property of plasticity affected region and irradiation depth of ion-irradiated materials based on the experimental data measured through cross-sectional nanoindentation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.