Abstract

A widely applicable solvothermal route to nanocrystalline iron, indium, gallium, and zinc oxide based on the reaction between the corresponding metal acetylacetonate as metal oxide precursor and benzylamine as solvent and reactant is presented. Detailed XRD, TEM, and Raman studies prove that, with the exception of the iron oxide system, where a mixture of the two phases magnetite and maghemite is formed, only phase pure materials are obtained, gamma-Ga(2)O(3), zincite ZnO, and cubic In(2)O(3). The particle sizes lie in the range of 15-20 nm for the iron, 10-15 nm for the indium, 2.5-3.5 nm for gallium, and around 20 nm for zinc oxide. GC-MS analysis of the final reaction solution after removal of the nanoparticles showed that the composition is rather complex consisting of more than eight different organic compounds. Based on the fact that N-isopropylidenebenzylamine, 4-benzylamino-3-penten-2-one, and N-benzylacetamide were the main species found, we propose a detailed formation mechanism encompassing solvolysis of the acetylacetonate ligand, involving C-C bond cleavage, as well as ketimine and aldol-like condensation steps.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.