Abstract

Controlled Suzuki–Miyaura coupling polymerization of 7′‐bromo‐9′,9′‐dioctyl‐fluoren‐2′‐yl‐4,4,5,5‐tetramethyl‐[1,3,2]dioxaborolane initiated by bromo(4‐tert‐butoxycarbonylamino‐phenyl)(tri‐tert‐butylphosphine)palladium (1) or bromo(4‐diethoxyphosphoryl‐phenyl)(tri‐tert‐butylphosphine)palladium (2) yields functionalized polyfluorenes (Mn = 4 × 103 g mol−1, Mw/Mn < 1.2) with a single amine or phosphonic acid, respectively, end‐group. High temperature synthesis of cadmium selenide quantum dots with these functionalized polyfluorenes as stabilizing ligands yields hybrid particles consisting of good quality (e.g. emission full width at half maximum of 30 nm; size distribution σ < 10%) inorganic nanocrystals with polyfluorene attached to the surface, as corroborated by transmission electron microscopy analysis and analytical ultracentrifugation. Sedimentation studies on particle dispersions show that a substantial portion (ca. half) of the phosphonic acid terminated polyfluorene ligands is bound to the inorganic nanocrystals, versus ca. 5% for the amino‐functionalized polyfluorene ligands. Single particle micro‐photoluminescence spectroscopy shows an efficient and complete energy transfer from the polyfluorene layer to the inorganic quantum dot.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.