A device for depositing silicon films from a sublimation source on standard silicon wafers with diameters of 52−100 mm is described. The source is a silicon single crystal heated to a preset temperature of 1300−1380°C. The uniform thickness and homogeneous doping over the wafer area are obtained by moving the sublimation source relative to the wafer.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.