Leachables of borosilicate glassware and silica-based anion exchange columns (QMAs) may influence nucleophilic substitution with [(18)F]fluoride ([(18)F]F(-)). Aluminum, boron and silicon, all constituents of borosilicate glass, were found as water soluble leachables in a typical PET synthesis setup. Relevant ranges of the leachable quantities were studied based on an experimental design, in which species of the three elements were added to the labeling of the precursor for anti-1-amino-3-[(18)F]fluorocyclobutyl-1-carboxylic acid ([(18)F]FACBC). Levels of 0.4-2 ppm aluminum as AlCl(3) had a strong negative influence on labeling yield while 4-20 ppm of boron as KBO(2) and 50-250 ppm of silicon as Na(2)SiO(3) did not have a significant impact. Interesting interaction effects between the elements were observed, where particularly KBO(2) reduced the negative effect of AlCl(3) on labeling yield. It can be concluded that leachables of borosilicate glassware easily can influence nucleophilic substitution with n.c.a. [(18)F]F(-) and give variable yields.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.