Abstract
To improve the service and machining performance of the workpiece, the tool wear mechanisms, surface machining quality, and wear resistance in conventional side milling (CSM) and longitudinal-torsional ultrasonic vibration side milling (LTUVSM) of GH4169 superalloy at different cutting lengths are investigated systematically. Tool wear mechanisms are revealed and the correlation between machined surface quality with tool wear is analyzed correspondingly. Tool wear patterns mainly include adhesive wear, diffusion wear, abrasive wear, and chipping sticking. Better surface quality is achieved in LTUVSM due to a maximum reduction of flank wear bandwidth and wear rate by 71.9% and 71.5%, respectively, compared to CSM. The friction coefficient, initial wear stage time, and wear volume of dry sliding wear were measured to evaluate the workpiece wear resistance. The maximum reductions in friction coefficient and wear volume in LTUVSM are 18.2% and 15.8% compared to CSM. The regular ultrasonic vibration textures suppress the friction and the growth of contact nodes in the contact area, decreasing the degree of surface wear, which is demonstrated by a 38.8% increase in initial wear stage time compared to CSM. In conclusion, the workpiece in LTUVSM exhibits higher wear resistance because of the improvement of tool wear and the guarantee of surface quality.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.