Abstract
A comparative study of O3 and H2O as oxidizers for atomic layer deposition (ALD) HfOx and AlOx thin films was carried out employing a 300-mm wafer capable ALD cluster tool. TEMAHf (tetrakis-ethylmethylamino-hafnium) and TMA (trimethyl-aluminium) were used as metal precursors. Process conditions were varied to evaluate the effects on unary metal oxide growth as an approach towards developing a mixed-phase binary metal oxide growth process. Films were characterized using scanning electron microscopy (SEM), x-ray photoelectron spectroscopy (XPS), Rutherford backscattering spectroscopy (RBS), and capacitance measurements of MOS capacitor structures. Initial testing results of the electrical properties of resulting binary metal oxides will be discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.