Abstract

In this paper, extensively experimental testing of fracture toughness for two different welded joints of API X80 pipeline steels after service were carried out. The microstructures and CTOD resistance curves of longitudinal submerged arc welded (LSAW) and spiral submerged arc welded (SSAW) joints were investigated at different locations of the base metal (BM), weld metal (WM) and heat affected zone (HAZ). The critical fracture toughness values were compared with each other. The optical microscope (OM), scanning electron microscope (SEM) and energy dispersive spectroscopy (EDS) were used to analyze the fracture mechanism and precipitates composition. This investigation will provide an important reference to engineering practice and evaluation of pipeline structures.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.