Abstract

Comparison of the conversion efficiency for efficient second-harmonic generation of Nd: YAG laser radiation is reported for KDP, LAP, KTP, BBO and LBO crystals. Conversion efficiencies as high as 50% and 46% were obtained for our laboratory-grown KDP and LAP crystals respectively, for power densities well below their damage thresholds.