Abstract

The use of a technological scheme which combines the processes of twisting and yarn heat-treatment makes it possible to intensify the process of textile grade polyester yarn manufacture as a result of shortening the series of textile-technology steps. The scheme permits one not only to set the twist well, but also to regulate the basic physicomechanical properties of the yarns over a wide range. By using the proposed technological scheme, depending on the assigned degree of deformation, one can obtained twisted yarns with a shrinkage of 1–2% at an initial elastic modulus up to 20 MPa.