Carboxylated chitin nanofibers were successfully prepared by direct surface TEMPO-mediated oxidation of chitin micro/nano fibers, that is, chitin was pulverized into various sizes by aqueous counter collision (ACC) with different pass numbers prior to carboxylation. Meanwhile, chitin nanofibers (ACC-ChNs) were successfully obtained using ACC pulverization applied to crab shell α-chitin. Surface oxidation gave oxidized-ACC-ChNs superior pH-responsive sol-gel transition properties. The combination of aqueous counter collision and TEMPO-mediated oxidation led to double oxidation efficiency of chitin nanofibers compared to oxidation of original non-ACC pulverized chitin. Notably, the carboxylate content of oxidized-ACC-ChNs reached 0.67–0.79 mmol/g after the ACC defibrillation followed by TEMPO/NaBr/NaClO oxidation, comparing to ~ 0.40 mmol/g of oxidized original (without ACC defibrillation) chitin when the same dosage of NaClO (2.5 mmol/g) was applied. The results proved that the nanofibrillation of chitin by ACC process effectively improved the oxidation efficiency. Thus controllable moderate oxidation with slight amount of NaClO avoided severe degradation caused by excessive NaClO used. The chemical, crystalline structures and the morphological properties of ACC-ChNs and oxidized ACC-ChNs was evaluated. Furthermore, the oxidized ACC-ChNs based hydrogels possessing improved storage modulus were successfully formed by gas phase coagulation process.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.