Abstract
A numerical analysis using cohesive zone model under cyclic loading is proposed to develop a coupled predictive approach of crack growth in single crystal. The process of material damage during fatigue crack growth is described using an irreversible cohesive zone model, which governs the separation of the crack flanks and eventually leads to the formation of free surfaces. The cohesive zone element is modeled to accumulate fatigue damage during loadings and no damage during unloadings. This paper presents the damage model and its application in the study of the crack growth for precracked specimens. The use of cohesive zone approach is validated through a convergence study. Then, a general procedure of parameters calibration is presented in pure fatigue crack growth. In the last section, an extension of the cohesive zone model is presented in the case of creep–fatigue regime at high temperature. The model showed its capability to predict with a good agreement the crack growth in the case of complex loading and complex specimen geometries.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.