Abstract

A recycling process is proposed in which spent cathode materials and Al foil are leached by low-concentration acids, then Al is selectively precipitated, finally the lithium iron phosphate material is synthesized by a one-step hydrothermal synthesis.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.