Accurate intracoronal castings can be produced using a castable ceramic--DICOR--for which there is a need to identify a suitable luting cement. The aim of this investigation was to evaluate the bond strength of three glass-ionomer luting cements and one resin cement to treated and untreated DICOR, enamel, and dentin surfaces. Forty "cerammed" DICOR specimens were assigned to four groups: (1-3) grit-blasting and bonding to each of the three glass-ionomer cements; and (4) acid-etching, silane coating, and bonding to the resin cement. Seventy enamel specimens were assigned to seven groups: (1-3) no etching and bonding to each of the glass-ionomer cements; (4-7) acid-etching and bonding to the glass-ionomer cements and the resin cement. Seventy dentin specimens were assigned to seven groups: (1-4) bonding to each of the three glass-ionomer cements and the resin cement; (5-7) polyacrylic acid preconditioning and bonding to each of the three glass-ionomer cements. The mean resin cement bond strengths (MN/m2) to DICOR (9.4) and to etched enamel (10.7) were significantly greater (p less than 0.01) than those of the glass-ionomer cements (DICOR, 0.8-1.2; enamel, 0.4-0.9). Preconditioning of enamel and dentin significantly increased (p less than 0.05) the bond strengths to the glass-ionomer cements. The mean bond strength of the resin cement to untreated dentin (4.3) was significantly higher (p less than 0.05) than the glass-ionomer bond strengths to untreated dentin (1.0-1.7) and to preconditioned dentin (2.1-3.3). The high bond strengths achieved with the resin cement are encouraging. Selected surface treatment of DICOR, enamel, and dentin prior to luting should be clinically useful.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call