Abstract : A bar impact test was developed to study the dynamic fracture responses of precracked ceramic bars, Al2O3 and 15/29% volume SiCw/Al2O3. Laser interferometric displacement gage data was used together with dynamic finite element analysis to determine the instantaneous crack length and the dynamic stress intensity factor, K sub ID(t), in the fracturing ceramic bars impacted with impactor velocities of 5.8, 8.0, and 10 m/s. The crack velocities increased from 1400 to 2600 m/s with increasing impact velocity. K sub ID(t) initiated at the expected dynamic fracture toughness and increased with time and with increasing impact velocity. The dynamic initiation fracture toughness and an increasing K sub ID(t) with time and increasing impact velocity were obtained.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.