Abstract

Coals (NCB rank 102 to 902) were co-carbonized with solvent-refined coals and coal extracts, mixing ratio of 7:3, to 873 K, heating at 10 K min−1 with a soak period of 1 h. Resultant cokes were examined in polished section using reflected polarized-light microscopy and optical textures were recorded photographically. These optical textures were compared to assess the ability of the additive pitch to modify both the size and extent of optical texture of resultant cokes. The objective of the study is to provide a fundamental understanding of the use of pitch materials in co-carbonizations of lower-rank coals to make metallurgical coke. A Gulf SRC was able to modify the optical texture of cokes from all coals except the anthracite. Soluble fractions of this Gulf SRC were less effective than the parent SRC. A coal extract (NCB D112) modified coke optical texture, the extent being enhanced as the rank of coal being extracted was increased. Hydrogenation of the coal extract increased the penetration of the pitch into the coal particles but simultaneously reduced the size of the optical texture relative to the non-hydrogenated pitch. This indicates a positive interaction of pitch with coal in the co-carbonization process. The optical texture of the cokes from the hydrogenated coal extract in single carbonizations was larger than that from the non-hydrogenated material. Mechanisms explaining these effects are briefly described.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call