Abstract
At high pressures or at low temperatures lubricating oils cause the solidification First, phase diagrams of paraffinic mineral oils (PN), traction oils (SN), polybutene (PB), DOS and BBPH were drawn in pressure-temperature plots of three different states (liquid, viscoelastic solid and elastic-plastic solid). Next, the four-ball tests were used to evaluate anti-wear characteristics of lubricating oils in boundary lubrication regime. The SNs showed the minimum wear scar in four-ball wear test The anti-wear characteristics of oils was closely related with EHL film thickness and the oil molecular packing parameter T_<VE>-T (T_<VE> : viscoelastic solid transition temperature at pressure p of wear test condition, T: oil temperature).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: The Proceedings of the Materials and processing conference
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.