Abstract
The forming process of millimeter or submillimeter shell parts using incremental sheet metal forming technique was tested. The formability of aluminium, copper and stainless steel foils into quadrangular pyramid-shaped shell parts were examined. In this process the pinhole defects were formed in the steeper wall and thin workpiece. In order to prevent the defect, new tool path in which the local strain concentration is controlled was proposed. By this tool path the steeper wall was formed successfully.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.