Abstract
To make clear the wear property of Fe-Al intermetallic compounds, the five specimens of Fe_3Al, FeAl, FeAl_2, Fe_2Al_5 and FeAl_3 were subjected to abrasion tests using abrasive paper with some grain size. In FeAl_2, Fe_2Al_5 and FeAl_3 specimens with relatively high Al composition, the wear surface translated from ductile wear surface into brittle wear surface with chipping at the specific size of abrasive grain. The effect of applied force per abrasive grain on this ductile-brittle transition was discussed from the relationship between micro cracking condition in indentation test and grain size on abrasive paper.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: The Proceedings of The Manufacturing & Machine Tool Conference
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.