Abstract As-received and chemically treated copper foams were characterized by means of laboratory X-ray tomography with a resolution of 0.5 μm. 3D image processing and analysis allowed the morphological parameters (size, sphericity, tortuosity etc.) of the pores and copper skeleton to be determined. The chemical dissolution of the Cu foam in an acid hydrogen peroxide solution results in an increase of the open pore size (from 54 to 93 μm) and a decrease of the foam thickness (from 140 to 115 μm). With an open porosity of 81.8% and a specific surface area as high as 280,000 (49,000) m2/m3 of Cu (foam), the chemically-treated Cu foam appears very attractive for use as a 3D current collector for metal (e.g. Si) based anodes for Li-ion batteries.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.