Nanostructured Mg-5%Al-x%Nd (x=0.5,1 and 5 wt.%) alloys were prepared by mechanical alloying. Microstructural characterisation revealed average crystalline size to be about 90 nm after sintering and extrusion. Mechanical properties showed increase in 0.2% yield stress, ultimate tensile strength and ductility after 20 h of mechanical alloying. The increase in yield stress and ultimate tensile strength was attributed to reduction in grain size as well as to the enhanced diffusion after mechanical activation. Although ultra high yield stress was observed from the specimen with 5%Nd, its ductility was reduced to about 1.6%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.