In this work, we report the 2.05μm emission and ∼3μm broadband spectra of Ho2O3-doped 33GeO2–30TeO2–27PbO–10CaO (in mol%) glass under 640nm laser excitation. Clear emission spectra due to the 5I7–5I8 transition and the 5I6–5I7 transition in Ho3+ are observed. The 2.05μm emission intensity and the full width at half maximum (FWHM) of the ∼3μm broadband depend on the Ho concentration. The peak stimulated emission cross-section of Ho3+ is 6.57×10−21cm2 at 2.05μm, as calculated by the McCumber theory. The emission spectra are recorded and the maximum emission intensity at 2.05μm is obtained at a doping level of 0.5mol% Ho2O3 in the glass. A broad and flat emission band from 2700nm to 3050nm is observed in 2mol% Ho2O3-doped tellurium germanate glass. The lifetime of the 5I7 state decreases with the increase in Ho3+ concentration due to non-radiative relaxation processes. An energy transfer coefficient of 271.88mol−1s−1 is obtained.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.