Abstract

For the first time, we demonstrated the fabrication of mechanically exfoliated molybdenum disulfide (MoS2) samples deposited onto a D-shaped optical fiber. The MoS2 exfoliated flakes were deposited onto a stacked of 1.2 µm PVA (polyvinyl alcohol) and 300 nm PMMA (polymethyl methacrylate) layers and then transferred directly onto a side polished surface of D-shaped optical fiber with polishing length of 17 mm and no distance from the fiber core. The sample exhibited a high polarization performance as a polarizer with relative polarization extinction ratio of 97.5%. By incorporating the sample as a saturable absorber in the Erbium-doped fiber laser (EDFL), bandwidth of 20.5 nm and pulse duration of 200 fs were generated, which corresponded to the best mode-locking results obtained for all-fiber MoS2 saturable absorber at 1.5 µm wavelength.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.