Abstract

The followings are the test results of the bead shaping in Lay Down Welding.1. All of the factors, viz. (1) kind of the covering, (2) the covering composition, (3) the eccentricity ratio of electrode, (4) arc current, (5) groove angle of base metal, and (6) welding position as welding conditions, influence on the bead shaping.2. As to the relation between 3 factors (the covering composition, the eccentricity ratio of electrode and arc current in welding condition) and good bead area in flat and horizontal fillet welding; By increasing iron powder in the coverings, decreasing the gas materials and enlarging the eccentricity ratio of electrode, the currency for good bead area becomes higher and the extent of current become enlarged. The good bead area in horizontal fillet welding become narrower as compared with the V groove (flat fillet) welding.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.