Abstract
The aim of this study was to develop a 2-N, 6-O-sulfated chitosan (26SCS) modified electrospun fibrous PCL scaffold for bone morphogenetic protein-2 (BMP-2) delivery to improve osteoinduction. The PCL scaffold was modified by an aminolysis reaction using ethylenediamine (ED) and 26SCS was immobilized via electrostatic interactions (PCL-N-S). Scaffolds were characterized by scanning electron microscopy (SEM), atomic force microscopy (AFM), X-ray photoelectron spectroscopy (XPS) and contact angle measurements. In vitro BMP-2 adsorption and release kinetics indicated that modified PCL-N-S scaffolds showed higher levels of binding of BMP-2 (about 30–100 times), moderative burst release (about one third), and prolonged releasing time compared to the unmodified PCL scaffold. The bioactivity of released BMP-2 determined by alkaline phosphatase (ALP) activity assay was maintained and improved 8–12 times with increasing concentration of immobilized 26SCS on the scaffolds. In vitro studies demonstrated that bone marrow mesenchymal stem cells (BMSCs) attached more readily to the PCL-N-S scaffolds with increased spreading. In conclusion, 26SCS modified PCL scaffolds can be a potent system for the sustained and bioactive delivery of BMP-2.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.