Abstract
AbstractA coating method and process of an anti‐smudge layer on the Anti‐Reflection (AR) film are described. Several kinds of solvents were tested to achieve a very thin anti‐smudge layer using a direct gravure coater. Solvents for the anti‐smudge reagent were required suitable boiling point good volubility and low surface energy. Fluorinated solvents, i‐Propanol (IPA), and IPA mixed organic solvents met the requirements.The addition of a catalyst prevented a back print, which was one of most important technical point for the roll‐to‐roll coating.The film thickness of 3.5 nm exhibited excellent anti‐smudge property and also did not sigficantly affect AR properties.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.