Abstract
The spark sintering technique is used for the sintering of 7075-rapidly solidified aluminum powder. The various microstructures are obtained by changing of process parameters, such as the maximum sintering temperature, sintering period and cooling method after sintering. The solid soluted amount of main alloying elements increases as the maximum temperature and period increase in the sintering. Various materials sintered at 873K for 10 to 2400 sec show the same behaviour of age-hardening. On the other hand, plastic strain of material increases as the holding period in the sintering at 873K increases, and that of materials sinterd at 873K for 1200sec is same as that of solution treated materials. It is suggested on the basis of value of the plastic strain obtained from tensile test that materials sintered under the conditions of the long exposure and higher temperatures show largely solid-soluted amount of main alloying elements and promotion of sintering.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.