Abstract

In this paper, fatigue strength of high-modulus (HM) type poly-p-phenylene benzobisoxazole (PBO) fiber improved tensile modules by heat-treatment have been investigate. To reveal the fatigue strength of fiber with different diameters, it is necessary to take into account the size effects on it in the diameter direction. In this report, such effect in the diameter direction is cut off from the experimental fatigue strength so as to evaluate is closely. As a result, variance in date on HM fiber stress ratios is small, and fatigue strength can be approximated to straight lines falling down from left to right on a single logarithm graph. Fatigue strength on stress ratio R=0.1 becomes lower than those of R=0.5, 0.7 and 1.0.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.