1.3 µm laser diodes with butt-jointed selectively grown spot-size converters have been successfully fabricated on a 2 in InP substrate. Their threshold current and far-field patterns were uniformly distributed over the 2 in wafer. These uniform characteristics were obtained by combining uniform MOVPE growth, wet etching, and CH4/H2 reactive ion etching.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.