Abstract
0-3 and 1-3 composites were fabricated using piezoelectric single crystals (PSCs). These two connectivities were specifically chosen for large area fabrication. In particular, a lamination technique was used for 1-3 piezocomposites instead of the standard ‘dice and fill’ method. For 0-3 connectivity, the thickness coupling factor of the fabricated materials using PSC phase was twice that obtained using standard PZT powder for the same volume fraction (60%). However, the efficiency of the poling remained low. For the 1-3 piezocomposites, the properties (such as the thickness coupling factor which reached 74%) of the samples fabricated by the lamination technique were comparable to those obtained with standard methods. Finally, three ultrasonic transducers with centre frequencies between 600 and 850 kHz were fabricated to evaluate the performance of these new piezoelectric composites.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.