Abstract

Splat-cooling technique with a cooling rate better than 106 K/s helps to increase the Pt solubility in the (cubic) γ-U phase and retain such γ-U phase in U-15 at.% Pt splat down to low temperatures. The splat-cooled U-Pt alloys are very stable in exposing to air. The γ-U phase (U-15 at.% Pt splat) is characterized by a negative temperature coefficient of the resistivity (dρ/dT < 0). The splats become superconducting below 1.1 K.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.