Abstract

Stainless steels are alloy steels with a nominal chromium content of at least 11 percent, with other alloy additions. The stainlessness and corrosion resistance of these alloy steels are attributed to the presence of a passive oxide film on the surface. When exposed to conditions like Resistance Spot Welding (RSW) process that remove the passive oxide film, stainless steels are subject to corrosive attack. And exposure to elevated temperatures causes oxidation (discoloration) of areas around indentation in Spot welding. In this paper, deal with the effect of shielding gas (Ar) preventing the corrosion, oxidation of stainless steel. And find the optimal shielding gas flow rate. In addition, suggest effective purging method for direct/indirect spot welding process.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.