Abstract

Mg-4.3Zn-0.7Y (at%) alloy powders were prepared using an industrial scale gas atomizer, followed by warm extrusion. The powders were almost spherical in shape. The microstructure of atomized powders and those extruded bars was examined using Scanning Electron Microscopy (SEM), Energy Dispersive X-ray Spectroscope (EDS) and X-ray Diffractometer (XRD). The grain size of the powders was coarsen as the initial powder size increased. After the extrusion, the grain size became fine due to the severe plastic deformation during the extrusion with the ratio of 10:1. Both the ultimate strength and elongation were enhanced with the decrease of initial particle size.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.